Text from PDF Page: 151

elution cycle, 59 mg of Li was lost during sweeping processes. And lastly, in the post-treatment with LiMnO particles, 17 mg of Li was lost during sweeping processes. In the overall process, 141 mg of Li was lost, which means that 69.2 % of the initially adsorbed lithium could be recovered in the final solution. The lithium concentrations, lithium to foreign ion ratio and lithium loss in each step were summarized in Table 3.59. Table 3.59 Li concentration, Li/foreign ion ratio, Li loss in each separation step starting from artificial brine Brine Initial brine After first ads.- sweep.-elut. cycle After second ads.- sweep.-elut. cycle After post treatment Na/Li K/Li Mg/Li 124,256 10,381 21,419 3.0 2.2 8.6 0.12 0.08 0.39 0.04 0.08 0.07 Li conc. (ppm) 0.43 27.4 261.0 1675.6 Li percantage among total cations (%) 6.408x10-4 6.8 62.7 84.0 TOTAL Li Loss (mg) - 65 59 17 141 Li Loss (%) - 14.2 12.9 3.7 30.8 A feasibility study of recovering lithium from the concentrated brine in Çamaltı Salina is given in APPENDIX D. 3.4.5.2 Efficiency of the overall process starting from clay extract In order to have 3217 ppm Li, 126.2 ppm Na, 83.8 ppm K and 233.1 ppm Mg in 100 ml of water, 2.23 L of clay extract was processed with a concentration of 412 ppm Li, 4964 ppm Na, 584 ppm K and 15972 ppm Mg. In the adsorption-sweeping- elution cycle, 642 mg Li was adsorbed, while 42 mg of Li was lost during sweeping process. In the post-treatment with LiMnO particles, 58.4 mg of Li was lost during sweeping processes. In the overall process, 100.4 mg of Li was lost, which means 127

PDF Image | SEPARATION OF LITHIUM FROM BRINES

separation-lithium-from-brines-151

PDF Search Title:

SEPARATION OF LITHIUM FROM BRINES

Original File Name Searched:

separation-lithium-from-brine.pdf

DIY PDF Search: Google It | Yahoo | Bing

Product and Development Focus for Infinity Turbine

ORC Waste Heat Turbine and ORC System Build Plans: All turbine plans are $10,000 each. This allows you to build a system and then consider licensing for production after you have completed and tested a unit.

Redox Flow Battery Technology: With the advent of the new USA tax credits for producing and selling batteries ($35/kW) we are focussing on a simple flow battery using shipping containers as the modular electrolyte storage units with tax credits up to $140,000 per system.

Our main focus is on the salt battery. This battery can be used for both thermal and electrical storage applications.

We call it the Cogeneration Battery or Cogen Battery.

One project is converting salt (brine) based water conditioners to simultaneously produce power.

In addition, there are many opportunities to extract Lithium from brine (salt lakes, groundwater, and producer water).

Salt water or brine are huge sources for lithium. Most of the worlds lithium is acquired from a brine source. It's even in seawater in a low concentration. Brine is also a byproduct of huge powerplants, which can now use that as an electrolyte and a huge flow battery (which allows storage at the source).

We welcome any business and equipment inquiries, as well as licensing our turbines for manufacturing.

CONTACT TEL: 608-238-6001 Email: greg@infinityturbine.com | RSS | AMP